ISO 286 · Shaft · 3–6 mm

h5 shaft tolerance, 3–6 mm

h5 tolerance for shafts over 3 up to 6 mm is 0 / −0.005 mm (0 / −0.00020 in). A 6 mm h5 shaft measures 5.995–6.000 mm; a 5 mm one, 4.995–5.000 mm. The table gives each common size in the range in mm and inches.

h5 shaft tolerance zone, 3–6 mm: es 0 µm, ei −5 µm against the zero line.es 0 µmei −5 µmtolerance zone h5zero line 3–6 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

h5 limits, over 3 up to 6 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

h5 deviations over 3 up to 6 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
3–60−50−0.0050−0.000205

Checked against 4 published copies

Common sizes, h5 shaft

The smallest and largest shaft each size allows. 3 mm itself belongs to the range below.

h5 smallest and largest size for common sizes over 3 up to 6 mm
SizeMin mmMax mmSize inMin inMax in
4 h53.9954.0000.15750.157280.15748
5 h54.9955.0000.19690.196650.19685
6 h55.9956.0000.23620.236020.23622

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4