ISO 286 · Shaft · 0–3 mm
h6 shaft tolerance, 0–3 mm
h6 tolerance for shafts over 0 up to 3 mm is 0 / −0.006 mm (0 / −0.00024 in). A 3 mm h6 shaft measures 2.994–3.000 mm; a 2 mm one, 1.994–2.000 mm. The table gives each common size in the range in mm and inches.
h6 limits, over 0 up to 3 mm
Deviations from the nominal size. Inches are the µm values ÷ 25,400.
| Size, mm | Upper µm | Lower µm | Upper mm | Lower mm | Upper in | Lower in | Band µm |
|---|---|---|---|---|---|---|---|
| 0–3 | 0 | −6 | 0 | −0.006 | 0 | −0.00024 | 6 |
Checked against 3 published copies
Common sizes, h6 shaft
The smallest and largest shaft each size allows.
| Size | Min mm | Max mm | Size in | Min in | Max in |
|---|---|---|---|---|---|
| 1 h6 | 0.994 | 1.000 | 0.0394 | 0.03913 | 0.03937 |
| 1.5 h6 | 1.494 | 1.500 | 0.0591 | 0.05882 | 0.05906 |
| 2 h6 | 1.994 | 2.000 | 0.0787 | 0.07850 | 0.07874 |
| 2.5 h6 | 2.494 | 2.500 | 0.0984 | 0.09819 | 0.09843 |
| 3 h6 | 2.994 | 3.000 | 0.1181 | 0.11787 | 0.11811 |
Checked against 3 published copies
ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page comes from the same engine as the h6 chart, checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)