ISO 286 · Shaft · 180–250 mm

h7 shaft tolerance, 180–250 mm

h7 tolerance for shafts over 180 up to 250 mm is 0 / −0.046 mm (0 / −0.00181 in). A 200 mm h7 shaft measures 199.954–200.000 mm; a 250 mm one, 249.954–250.000 mm. The table gives each common size in the range in mm and inches.

h7 shaft tolerance zone, 180–250 mm: es 0 µm, ei −46 µm against the zero line.es 0 µmei −46 µmtolerance zone h7zero line 180–250 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

h7 limits, over 180 up to 250 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

h7 deviations over 180 up to 250 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
180–2500−460−0.0460−0.0018146

Checked against 4 published copies

Common sizes, h7 shaft

The smallest and largest shaft each size allows. 180 mm itself belongs to the range below.

h7 smallest and largest size for common sizes over 180 up to 250 mm
SizeMin mmMax mmSize inMin inMax in
200 h7199.954200.0007.87407.872207.87402
220 h7219.954220.0008.66148.659618.66142
250 h7249.954250.0009.84259.840719.84252

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4