ISO 286 · Shaft · 50–80 mm

h7 shaft tolerance, 50–80 mm

h7 tolerance for shafts over 50 up to 80 mm is 0 / −0.030 mm (0 / −0.00118 in). A 60 mm h7 shaft measures 59.970–60.000 mm; an 80 mm one, 79.970–80.000 mm. The table gives each common size in the range in mm and inches.

h7 shaft tolerance zone, 50–80 mm: es 0 µm, ei −30 µm against the zero line.es 0 µmei −30 µmtolerance zone h7zero line 50–80 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

h7 limits, over 50 up to 80 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

h7 deviations over 50 up to 80 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
50–800−300−0.0300−0.0011830

Checked against 4 published copies

Common sizes, h7 shaft

The smallest and largest shaft each size allows. 50 mm itself belongs to the range below.

h7 smallest and largest size for common sizes over 50 up to 80 mm
SizeMin mmMax mmSize inMin inMax in
55 h754.97055.0002.16542.164172.16535
60 h759.97060.0002.36222.361022.36220
65 h764.97065.0002.55912.557872.55906
70 h769.97070.0002.75592.754722.75591
75 h774.97075.0002.95282.951572.95276
80 h779.97080.0003.14963.148433.14961

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4