js7 tolerance on a 25 mm shaft is +0.0105 / −0.0105 mm, so the shaft measures 24.9895–25.0105 mm. A js shaft’s band sits evenly on both sides of the nominal size, ± half the IT grade. Grade 7 (IT7) sets the band’s width; the chart below gives it for every size to 500 mm.
JS7 hole on 25 mm: +0.0105 / −0.0105 mm. JS7 hole tolerance
Limits by size
Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.
| Size, mm | Upper µm | Lower µm | Upper in | Lower in |
|---|---|---|---|---|
| 0–3 | +5 | −5 | +0.00020 | −0.00020 |
| 3–6 | +6 | −6 | +0.00024 | −0.00024 |
| 6–10 | +7.5 | −7.5 | +0.00030 | −0.00030 |
| 10–18 | +9 | −9 | +0.00035 | −0.00035 |
| 18–30 | +10.5 | −10.5 | +0.00041 | −0.00041 |
| 30–50 | +12.5 | −12.5 | +0.00049 | −0.00049 |
| 50–80 | +15 | −15 | +0.00059 | −0.00059 |
| 80–120 | +17.5 | −17.5 | +0.00069 | −0.00069 |
| 120–180 | +20 | −20 | +0.00079 | −0.00079 |
| 180–250 | +23 | −23 | +0.00091 | −0.00091 |
| 250–315 | +26 | −26 | +0.00102 | −0.00102 |
| 315–400 | +28.5 | −28.5 | +0.00112 | −0.00112 |
| 400–500 | +31.5 | −31.5 | +0.00124 | −0.00124 |
Checked against 4 published copies
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)