ISO 286 · Shaft

k11 shaft tolerance

k11 tolerance on a 25 mm shaft is +0.130 / 0 mm, so the shaft measures 25.000–25.130 mm. A k shaft sits above the nominal size, for transition and interference fits in an H hole. Grade 11 (IT11) sets the band’s width; the chart below gives it for every size to 500 mm.

k11 shaft tolerance zone for every size range from 0–3 mm to 400–500 mm, against the zero line; 18–30 mm is +130 / 0 µm.tolerance zone k11, 18–30 mm: +130 / 0 µmsize range 0–3 to 400–500 mm
One band per size range against the zero line. The marked band holds 25 mm. Deviations to scale; the size ranges are evenly spaced, not to scale.

Limits by size

Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.

k11 limits by nominal size
Size, mmUpper µmLower µmUpper inLower in
0–3+600+0.002360
3–6+750+0.002950
6–10+900+0.003540
10–18+1100+0.004330
18–30+1300+0.005120
30–50+1600+0.006300
50–80+1900+0.007480
80–120+2200+0.008660
120–180+2500+0.009840
180–250+2900+0.011420
250–315+3200+0.012600
315–400+3600+0.014170
400–500+4000+0.015750

Checked against 3 published copies

Any size and fit in the calculator

Sources

Sources3