ISO 286 · Shaft · 180–250 mm
k5 shaft tolerance, 180–250 mm
k5 tolerance for shafts over 180 up to 250 mm is +0.024 / +0.004 mm (+0.00094 / +0.00016 in). A 200 mm k5 shaft measures 200.004–200.024 mm; a 250 mm one, 250.004–250.024 mm. The table gives each common size in the range in mm and inches.
k5 limits, over 180 up to 250 mm
Deviations from the nominal size. Inches are the µm values ÷ 25,400.
| Size, mm | Upper µm | Lower µm | Upper mm | Lower mm | Upper in | Lower in | Band µm |
|---|---|---|---|---|---|---|---|
| 180–250 | +24 | +4 | +0.024 | +0.004 | +0.00094 | +0.00016 | 20 |
Checked against 4 published copies
Common sizes, k5 shaft
The smallest and largest shaft each size allows. 180 mm itself belongs to the range below.
| Size | Min mm | Max mm | Size in | Min in | Max in |
|---|---|---|---|---|---|
| 200 k5 | 200.004 | 200.024 | 7.8740 | 7.87417 | 7.87496 |
| 220 k5 | 220.004 | 220.024 | 8.6614 | 8.66157 | 8.66236 |
| 250 k5 | 250.004 | 250.024 | 9.8425 | 9.84268 | 9.84346 |
Checked against 4 published copies
ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page comes from the same engine as the k5 chart, checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)