ISO 286 · Shaft · 3–6 mm
m6 shaft tolerance, 3–6 mm
m6 tolerance for shafts over 3 up to 6 mm is +0.012 / +0.004 mm (+0.00047 / +0.00016 in). A 6 mm m6 shaft measures 6.004–6.012 mm; a 5 mm one, 5.004–5.012 mm. The table gives each common size in the range in mm and inches.
m6 limits, over 3 up to 6 mm
Deviations from the nominal size. Inches are the µm values ÷ 25,400.
| Size, mm | Upper µm | Lower µm | Upper mm | Lower mm | Upper in | Lower in | Band µm |
|---|---|---|---|---|---|---|---|
| 3–6 | +12 | +4 | +0.012 | +0.004 | +0.00047 | +0.00016 | 8 |
Checked against 4 published copies
Common sizes, m6 shaft
The smallest and largest shaft each size allows. 3 mm itself belongs to the range below.
| Size | Min mm | Max mm | Size in | Min in | Max in |
|---|---|---|---|---|---|
| 4 m6 | 4.004 | 4.012 | 0.1575 | 0.15764 | 0.15795 |
| 5 m6 | 5.004 | 5.012 | 0.1969 | 0.19701 | 0.19732 |
| 6 m6 | 6.004 | 6.012 | 0.2362 | 0.23638 | 0.23669 |
Checked against 4 published copies
ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page comes from the same engine as the m6 chart, checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)