ISO 286 · Shaft

n5 shaft tolerance

n5 tolerance on a 25 mm shaft is +0.024 / +0.015 mm, so the shaft measures 25.015–25.024 mm. An n shaft sits above the nominal size, for transition and interference fits in an H hole. Grade 5 (IT5) sets the band’s width; the chart below gives it for every size to 500 mm.

n5 shaft tolerance zone for every size range from 0–3 mm to 400–500 mm, against the zero line; 18–30 mm is +24 / +15 µm.tolerance zone n5, 18–30 mm: +24 / +15 µmsize range 0–3 to 400–500 mm
One band per size range against the zero line. The marked band holds 25 mm. Deviations to scale; the size ranges are evenly spaced, not to scale.

Limits by size

Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.

n5 limits by nominal size
Size, mmUpper µmLower µmUpper inLower in
0–3+8+4+0.00031+0.00016
3–6+13+8+0.00051+0.00031
6–10+16+10+0.00063+0.00039
10–18+20+12+0.00079+0.00047
18–30+24+15+0.00094+0.00059
30–50+28+17+0.00110+0.00067
50–80+33+20+0.00130+0.00079
80–120+38+23+0.00150+0.00091
120–180+45+27+0.00177+0.00106
180–250+51+31+0.00201+0.00122
250–315+57+34+0.00224+0.00134
315–400+62+37+0.00244+0.00146
400–500+67+40+0.00264+0.00157