ISO 286 · Hole
P7 hole tolerance
P7 tolerance on a 25 mm hole is −0.014 / −0.035 mm, so the hole measures 24.965–24.986 mm. A P hole sits at or below the nominal size, for transition and interference fits on an h shaft. Grade 7 (IT7) sets the band’s width; the chart below gives it for every size to 500 mm.
p7 shaft on 25 mm: +0.043 / +0.022 mm. p7 shaft tolerance
Limits by size
Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.
| Size, mm | Upper µm | Lower µm | Upper in | Lower in |
|---|---|---|---|---|
| 0–3 | −6 | −16 | −0.00024 | −0.00063 |
| 3–6 | −8 | −20 | −0.00031 | −0.00079 |
| 6–10 | −9 | −24 | −0.00035 | −0.00094 |
| 10–18 | −11 | −29 | −0.00043 | −0.00114 |
| 18–30 | −14 | −35 | −0.00055 | −0.00138 |
| 30–50 | −17 | −42 | −0.00067 | −0.00165 |
| 50–80 | −21 | −51 | −0.00083 | −0.00201 |
| 80–120 | −24 | −59 | −0.00094 | −0.00232 |
| 120–180 | −28 | −68 | −0.00110 | −0.00268 |
| 180–250 | −33 | −79 | −0.00130 | −0.00311 |
| 250–315 | −36 | −88 | −0.00142 | −0.00346 |
| 315–400 | −41 | −98 | −0.00161 | −0.00386 |
| 400–500 | −45 | −108 | −0.00177 | −0.00425 |
Checked against 4 published copies
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)