ISO 286 · Shaft

s8 shaft tolerance

s8 tolerance on a 25 mm shaft is +0.068 / +0.035 mm, so the shaft measures 25.035–25.068 mm. An s shaft sits above the nominal size, for transition and interference fits in an H hole. Grade 8 (IT8) sets the band’s width; the chart below gives it for every size to 500 mm.

s8 shaft tolerance zone for every size range from 0–3 mm to 450–500 mm, against the zero line; 18–30 mm is +68 / +35 µm.tolerance zone s8, 18–30 mm: +68 / +35 µmsize range 0–3 to 450–500 mm
One band per size range against the zero line. The marked band holds 25 mm. Deviations to scale; the size ranges are evenly spaced, not to scale.

Limits by size

Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.

s8 limits by nominal size
Size, mmUpper µmLower µmUpper inLower in
0–3+28+14+0.00110+0.00055
3–6+37+19+0.00146+0.00075
6–10+45+23+0.00177+0.00091
10–18+55+28+0.00217+0.00110
18–30+68+35+0.00268+0.00138
30–50+82+43+0.00323+0.00169
50–65+99+53+0.00390+0.00209
65–80+105+59+0.00413+0.00232
80–100+125+71+0.00492+0.00280
100–120+133+79+0.00524+0.00311
120–140+155+92+0.00610+0.00362
140–160+163+100+0.00642+0.00394
160–180+171+108+0.00673+0.00425
180–200+194+122+0.00764+0.00480
200–225+202+130+0.00795+0.00512
225–250+212+140+0.00835+0.00551
250–280+239+158+0.00941+0.00622
280–315+251+170+0.00988+0.00669
315–355+279+190+0.01098+0.00748
355–400+297+208+0.01169+0.00819
400–450+329+232+0.01295+0.00913
450–500+349+252+0.01374+0.00992

Checked against 3 published copies

Any size and fit in the calculator

Sources

Sources3