Tooling · Toolholder shanks
BT50 dimensions
A BT50 holder has a 69.85 mm (2.750") gauge diameter on a 7:24 taper, a 100.00 mm (3.937") flange 3.00 mm in front of the gauge line, and takes an M24 retention knob. CAT50 shares the taper and gauge diameter but has a 3.875" V-flange and a 1-8 UNC knob, so the two don’t swap on a tool changer.
BT50 shank
- Gauge (gauge-line) diameter
- 69.85 mm (2.750")
Two published copies agree
- Flange diameter
- 100.00 mm (3.937")
Two published copies agree
- Flange face in front of the gauge line
- 3.00 mm (0.118")
Two published copies agree
- Gauge line to the end of the taper
- 101.80 mm (4.008")
Two published copies agree
- Retention knob (pull stud) thread
- M24
Two published copies agree
- Taper
- 7:24 (3.500" per foot on diameter), shared by NMTB, CAT, BT and ISO/DIN steep tapers
Two published copies agree
- Retention knob profile (angle, length)
- Not given: it’s set by the machine builder, not the taper. Your machine’s manual names the knob.
Retention knob torque
| Maker | Torque |
|---|---|
| Techniks | 99 ft·lb (134 N·m), its own 50-taper knobs One source: Techniks, its own retention knobs |
| Rego-Fix | 100 N·m (74 ft·lb) at most, or the taper can deform One source: Rego-Fix, its maximum for any steep taper this size |
The two makers are about 2× apart, and Rego-Fix’s figure is a ceiling: a knob torqued too hard stretches the holder’s taper and it no longer seats true. Use your knob maker’s figure, and your machine builder’s if it gives one.
Why CAT and BT don’t swap
Show
The taper and its gauge diameter are the same, so a BT holder will seat in a CAT spindle by hand with the right knob. But the flange, the V-groove the tool changer grips and the drive slots differ, and the knob threads are inch on CAT and metric on BT, so a mixed holder doesn’t work in a tool changer. Steep tapers aren’t self-holding: the drawbar pulls the knob, and the drive keys, not the taper, carry the torque.
Sources4
- ToolholderExchange, BT tool holders: BT30, BT40 and BT50 dimensions (archived Apr 10, 2026)
- Vertex, MAS BT shank specification (D1, L1, t2, d1, G) (archived Nov 16, 2026)
- Techniks, torque specifications chart (retention knobs) (archived Jun 26, 2024)
- Rego-Fix, maximum torques for retention knobs (steep taper)