Drill breaks
Mitsubishi and OSG both say: lower the feed.
What you see
The drill snaps in the hole, or twists off at the shank.
Causes and what to change
Every fix here is from Mitsubishi and OSG's troubleshooting guides, unless marked. Change one thing at a time.
Flutes longer than the hole needs
Use a drill with shorter flutes
Only Mitsubishi
Feed too high
Lower the feed
Work it out: Drilling speeds and feeds calculator
Runout at the holder
Check runout at the holder and correct it
Only Mitsubishi
A machine, drill or setup that isn’t stiff, or work that moves
Make the machine, the drill and the work clamping stiffer
Only OSG
Relief ground too small
Regrind the point correctly
Only OSG
A worn drill
Regrind the worn drill
Only OSG
Chips packing in the flutes
Use a drill made to clear chips (wide flute, high helix or coolant through), or peck the hole
Only OSG
Work it out: Drilling speeds and feeds calculator
The drill struggling to enter the work
Spot the hole first, use a point thinning that cuts with less force, and clamp the work stiffer
Only OSG
Work it out
Often comes with
Sources
Sources2
- Mitsubishi Materials — Drilling course: Trouble shooting
- OSG — Drilling Technical Guide, Part 8: Troubleshooting (pp. 34–35)
Written in our own words from each maker's troubleshooting guide.