Chipped or notched edges
Sandvik, Harvey, OSG and Kennametal all say: lower the feed, most of all as the tool enters the cut; make the setup stiffer: the part, the holder and the tool.
What you see
Small chips missing along the edge or corner, cracks across the edge, or a notch worn in at the depth-of-cut line.
Causes and what to change
Every fix here is from Sandvik, Harvey, OSG and Kennametal's troubleshooting guides, unless marked. Change one thing at a time.
Feed too heavy, most of all as the tool enters the cut
Lower the feed, most of all as the tool enters the cut
Work it out: Chip load and feed rate calculatorTake a lighter cut
Only Harvey and OSG
A setup that isn’t stiff
Make the setup stiffer: the part, the holder and the tool
Chips cut a second time
Blow the chips clear so they aren’t cut twice
Only Sandvik, OSG and Kennametal
Runout, or a loose insert
Check runout, the cutter mounting and the insert screws
Only Harvey, OSG and Kennametal
Coolant hitting a hot edge on and off (heat cracks)
For heat cracks: keep the coolant steady, flooded or shut off
OSG suggests air or mist instead.
Only Sandvik, OSG and Kennametal
Scale, a work-hardened skin or a tough alloy at the depth-of-cut line (notching)
For a notch at the depth-of-cut line: lower the speed, use a lead-angle or round insert, and vary the depth
Only Sandvik and Kennametal
Other changes the makers name
Use a tougher grade or a stronger edge: a hone, T-land or corner radius
Only Sandvik, OSG and Kennametal
Where makers disagree
These point opposite ways, so they aren’t in a row above. If the changes above don’t cure it, try one side and watch.
On the grade for notching
- A tougher grade — Sandvik
- A more wear-resistant grade — Kennametal
Work it out
- Milling speeds and feeds calculator· a starting speed, feed and depth for your end mill
- Chip load and feed rate calculator· the feed rate for a chip load per tooth
Often comes with
Sources
Sources5
- Sandvik Coromant — Troubleshooting milling (archived Mar 22, 2026)
- Harvey Performance — End mill troubleshooting guide (archived Jul 22, 2024)
- OSG — Milling Technical Guide, 7: Troubleshooting and solutions (pp. 80–81) (archived Oct 26, 2025)
- Kennametal — Essential tips for troubleshooting indexable milling (archived Nov 12, 2026)
- Kennametal — Reducing chatter and vibration in end milling
Written in our own words from each maker's troubleshooting guide.