SAE J429 · UNF

1-1/4-12 UNF bolt torque

1-1/4-12 UNF Grade 5: 1,241 ft·lb dry, 930 ft·lb lubricated, for a steel bolt tightened to 75% of its proof load.

A 1-1/4-12 UNF Grade 5 bolt clamping two plates, in section: the head and the nut squeeze the joint with the clamp load.clamp load 59,548 lbfbolt 1-1/4-12 UNF Grade 5jointnut
1-1/4-12 UNF Grade 5 at 75% of its proof load. Not to scale.

Tightening torque

1-1/4-12 UNF tightening torque by grade, dry and lubricated
GradeDry ft·lbLubed ft·lbDry N·mLubed N·mClamp load
Grade 255341575056326,555 lbf
Grade 51,2419301,6821,26259,548 lbf
Grade 82,0121,5092,7282,04696,565 lbf

From the standard, ASME B1.1 tensile stress area

1 ft·lb = 1.355818 N·m. Lubricated is about 75% of dry (K 0.15 vs 0.20) for the same clamp load.

What these values assume

The preload, the nut factor and the formula
  • Clamp load is 75% of the proof load of the bolt's grade (SAE J429, ISO 898-1), the usual preload for a reusable joint.
  • Dry: K = 0.20, plain steel threads as received. Lubricated: K = 0.15, oiled threads. Plated, waxed or thread-locked threads take a different K and less torque.
  • Torque T = K × D × F, D the nominal diameter, F the clamp load; tensile stress area from ASME B1.1 or ISO 898-1.
  • Steel bolt and nut (or tapped hole) at least as strong as the bolt. Tapped aluminum or cast iron needs less.

Two published copies agree

A starting value, not a spec. Torque is only an indirect measure of clamp load: thread and under-head friction decide how much of it becomes clamp. The joint designer's or equipment maker's torque wins.

Published charts

What published charts print for 1-1/4-12 UNF

Dry, on the same basis (75% of proof, K 0.20), in ft·lb.

Grade 2
Fewer than two published charts print this size; the torque above is the formula's.
Grade 5
Fewer than two published charts print this size; the torque above is the formula's.
Grade 8
Fewer than two published charts print this size; the torque above is the formula's.

How it's worked

The arithmetic for Grade 5

As = .7854 × (1.2500 − .9743 / 12)² = 1.0729 in². Grade 5: F = .75 × 1.0729 × 74,000 psi = 59,548 lbf; dry T = .20 × 1.2500 × 59,548 / 12 = 1,241 ft·lb.

Sources