Bolt torque chart

A 1/2-13 grade 5 bolt takes 75.4 ft·lb dry or 56.5 ft·lb lubricated, and grade 8 takes 106 ft·lb dry, at 75% of proof load (T = K × D × F). Every size and grade is below; each size's page adds N·m, the clamp load and what published charts print.

Worked from each grade's proof load the way Fastenal, Portland Bolt and other published charts work theirs.

Bolt torque calculator: any thread, 90% of proof, your own K, or the clamp a torque gives

What these values assume

The preload, the nut factor and the formula
  • Clamp load is 75% of the proof load of the bolt's grade (SAE J429, ISO 898-1), the usual preload for a reusable joint.
  • Dry: K = 0.20, plain steel threads as received. Lubricated: K = 0.15, oiled threads. Plated, waxed or thread-locked threads take a different K and less torque.
  • Torque T = K × D × F, D the nominal diameter, F the clamp load; tensile stress area from ASME B1.1 or ISO 898-1.
  • Steel bolt and nut (or tapped hole) at least as strong as the bolt. Tapped aluminum or cast iron needs less.

Two published copies agree

A starting value, not a spec. Torque is only an indirect measure of clamp load: thread and under-head friction decide how much of it becomes clamp. The joint designer's or equipment maker's torque wins.

Inch bolts (SAE J429), ft·lb

Each cell: dry, with lubricated below it in smaller type.

SAE J429 grades: dry and lubricated torque in ft·lb
BoltGrade 2Grade 5Grade 8
1/4-20 UNC5.5lubricated 4.18.5lubricated 6.311.9lubricated 8.9
1/4-28 UNF6.3lubricated 4.79.7lubricated 7.213.6lubricated 10.2
5/16-18 UNC11.3lubricated 8.417.4lubricated 13.124.6lubricated 18.4
5/16-24 UNF12.5lubricated 9.419.3lubricated 14.527.2lubricated 20.4
3/8-16 UNC20.0lubricated 15.030.9lubricated 23.243.6lubricated 32.7
3/8-24 UNF22.6lubricated 17.035.0lubricated 26.249.4lubricated 37.1
7/16-14 UNC32.0lubricated 24.049.4lubricated 37.169.8lubricated 52.3
7/16-20 UNF35.7lubricated 26.855.2lubricated 41.477.9lubricated 58.4
1/2-13 UNC48.8lubricated 36.675.4lubricated 56.5106lubricated 79.8
1/2-20 UNF55.0lubricated 41.285.0lubricated 63.7120lubricated 90.0
9/16-12 UNC70.4lubricated 52.8109lubricated 81.6154lubricated 115
9/16-18 UNF78.5lubricated 58.9121lubricated 91.0171lubricated 128
5/8-11 UNC97.1lubricated 72.8150lubricated 113212lubricated 159
5/8-18 UNF110lubricated 82.5170lubricated 127240lubricated 180
3/4-10 UNC172lubricated 129267lubricated 200376lubricated 282
3/4-16 UNF192lubricated 144297lubricated 223420lubricated 315
7/8-9 UNC167lubricated 125429lubricated 322606lubricated 455
7/8-14 UNF184lubricated 138474lubricated 355669lubricated 502
1-8 UNC250lubricated 187644lubricated 483909lubricated 681
1-12 UNF274lubricated 205704lubricated 528995lubricated 746
1-1/8-7 UNC354lubricated 266794lubricated 5961,288lubricated 966
1-1/8-12 UNF397lubricated 298890lubricated 6681,444lubricated 1,083
1-1/4-7 UNC500lubricated 3751,121lubricated 8401,817lubricated 1,363
1-1/4-12 UNF553lubricated 4151,241lubricated 9302,012lubricated 1,509
1-3/8-6 UNC655lubricated 4911,469lubricated 1,1022,382lubricated 1,786
1-3/8-12 UNF746lubricated 5591,672lubricated 1,2542,712lubricated 2,034
1-1/2-6 UNC869lubricated 6521,950lubricated 1,4623,162lubricated 2,371
1-1/2-12 UNF978lubricated 7342,194lubricated 1,6453,557lubricated 2,668

Metric bolts (ISO 898-1), N·m

Each cell: dry, with lubricated below it in smaller type.

ISO 898-1 classes: dry and lubricated torque in N·m
BoltClass 8.8Class 10.9Class 12.9
M5 × 0.86.2lubricated 4.68.8lubricated 6.610.3lubricated 7.7
M6 × 110.5lubricated 7.915.0lubricated 11.317.6lubricated 13.2
M8 × 1.2525.5lubricated 19.136.5lubricated 27.342.6lubricated 32.0
M10 × 1.550.5lubricated 37.872.2lubricated 54.184.4lubricated 63.3
M12 × 1.7588.0lubricated 66.0126lubricated 94.4147lubricated 110
M14 × 2141lubricated 105201lubricated 151235lubricated 176
M16 × 2218lubricated 164312lubricated 234365lubricated 274
M18 × 2.5312lubricated 234431lubricated 323504lubricated 378
M20 × 2.5441lubricated 330610lubricated 457712lubricated 534
M22 × 2.5601lubricated 451831lubricated 623971lubricated 728
M24 × 3761lubricated 5711,053lubricated 7901,231lubricated 923
M27 × 31,116lubricated 8371,544lubricated 1,1581,805lubricated 1,354
M30 × 3.51,514lubricated 1,1352,094lubricated 1,5702,447lubricated 1,835
M33 × 3.52,060lubricated 1,5452,849lubricated 2,1373,330lubricated 2,498
M36 × 42,646lubricated 1,9853,661lubricated 2,7454,278lubricated 3,208
M8 × 127.3lubricated 20.439.0lubricated 29.345.6lubricated 34.2
M10 × 1.2553.2lubricated 39.976.2lubricated 57.189.0lubricated 66.8
M10 × 156.1lubricated 42.180.3lubricated 60.293.8lubricated 70.4
M12 × 1.592.0lubricated 69.0132lubricated 98.7154lubricated 115
M12 × 1.2596.1lubricated 72.1138lubricated 103161lubricated 121
M14 × 1.5152lubricated 114217lubricated 163254lubricated 190
M16 × 1.5233lubricated 175333lubricated 250389lubricated 292
M18 × 2331lubricated 248458lubricated 343535lubricated 401
M18 × 1.5350lubricated 263485lubricated 363566lubricated 425
M20 × 2464lubricated 348642lubricated 482751lubricated 563
M20 × 1.5489lubricated 367676lubricated 507790lubricated 593
M22 × 2630lubricated 472871lubricated 6531,018lubricated 764
M22 × 1.5659lubricated 495912lubricated 6841,066lubricated 800
M24 × 2830lubricated 6231,149lubricated 8611,342lubricated 1,007
M27 × 21,205lubricated 9031,666lubricated 1,2501,948lubricated 1,461
M30 × 21,677lubricated 1,2582,320lubricated 1,7402,712lubricated 2,034
M33 × 22,260lubricated 1,6953,126lubricated 2,3443,653lubricated 2,740
M36 × 32,802lubricated 2,1023,877lubricated 2,9074,531lubricated 3,398
Sources11