5/8-18 UNF bolt torque
5/8-18 UNF Grade 5: 170 ft·lb dry, 127 ft·lb lubricated, for a steel bolt tightened to 75% of its proof load.
Tightening torque
| Grade | Dry ft·lb | Lubed ft·lb | Dry N·m | Lubed N·m | Clamp load |
|---|---|---|---|---|---|
| Grade 2 | 110 | 82.5 | 149 | 112 | 10,558 lbf |
| Grade 5 | 170 | 127 | 230 | 173 | 16,317 lbf |
| Grade 8 | 240 | 180 | 325 | 244 | 23,036 lbf |
From the standard, ASME B1.1 tensile stress area
1 ft·lb = 1.355818 N·m. Lubricated is about 75% of dry (K 0.15 vs 0.20) for the same clamp load.
What these values assume
The preload, the nut factor and the formula
- Clamp load is 75% of the proof load of the bolt's grade (SAE J429, ISO 898-1), the usual preload for a reusable joint.
- Dry: K = 0.20, plain steel threads as received. Lubricated: K = 0.15, oiled threads. Plated, waxed or thread-locked threads take a different K and less torque.
- Torque T = K × D × F, D the nominal diameter, F the clamp load; tensile stress area from ASME B1.1 or ISO 898-1.
- Steel bolt and nut (or tapped hole) at least as strong as the bolt. Tapped aluminum or cast iron needs less.
Two published copies agree
A starting value, not a spec. Torque is only an indirect measure of clamp load: thread and under-head friction decide how much of it becomes clamp. The joint designer's or equipment maker's torque wins.
Published charts
What published charts print for 5/8-18 UNF
Dry, on the same basis (75% of proof, K 0.20), in ft·lb.
- Grade 2
- Fewer than two published charts print this size; the torque above is the formula's.
- Grade 5
- 170 ft·lbOnly two makers publish this: Fastenal and AIMS Industrial
- Grade 8
- 240 ft·lbOnly two makers publish this: Fastenal and AIMS Industrial
Only two makers publish this: Fastenal and AIMS Industrial
How it's worked
The arithmetic for Grade 5
As = .7854 × (0.6250 − .9743 / 18)² = 0.2560 in². Grade 5: F = .75 × 0.2560 × 85,000 psi = 16,317 lbf; dry T = .20 × 0.6250 × 16,317 / 12 = 170 ft·lb.
Sources
Sources8
- Portland Bolt — Strength requirements by grade (SAE J429) (archived May 11, 2026)
- Fastenal — Mechanical properties of inch fasteners (SAE J429) (archived Nov 11, 2026)
- Fastenal — Torque-tension relationship for A307A, Grade 5, 8 and 9 bolts (Rev 3-6-09) (archived Jul 12, 2023)
- Fastenal — Torque-tension relationship, ISO 898-1 classes 4.6, 8.8, 10.9 and 12.9, coarse thread (Jan 2016) (archived Oct 26, 2026)
- Portland Bolt — Bolt torque chart (75% of proof load) (archived Jul 22, 2026)
- AIMS Industrial — Imperial bolt torque chart (SAE J429) (archived Nov 13, 2026)
- AIMS Industrial — Metric bolt torque chart (ISO 898-1) (archived Nov 13, 2026)
- Engineers Edge — Torque vs tension for SAE J429 bolts (archived Oct 15, 2024)