ISO 898-1 · coarse

M18 × 2.5 bolt torque

M18 × 2.5 Class 10.9: 431 N·m dry, 323 N·m lubricated, for a steel bolt tightened to 75% of its proof load.

A M18 × 2.5 Class 10.9 bolt clamping two plates, in section: the head and the nut squeeze the joint with the clamp load.clamp load 119.8 kNbolt M18 × 2.5 Class 10.9jointnut
M18 × 2.5 Class 10.9 at 75% of its proof load. Not to scale.

Tightening torque

M18 × 2.5 tightening torque by grade, dry and lubricated
GradeDry N·mLubed N·mDry ft·lbLubed ft·lbClamp load
Class 8.831223423017286.6 kN
Class 10.9431323318239119.8 kN
Class 12.9504378372279140.0 kN

From the standard, ISO 898-1 tensile stress area

1 ft·lb = 1.355818 N·m. Lubricated is about 75% of dry (K 0.15 vs 0.20) for the same clamp load.

What these values assume

The preload, the nut factor and the formula
  • Clamp load is 75% of the proof load of the bolt's grade (SAE J429, ISO 898-1), the usual preload for a reusable joint.
  • Dry: K = 0.20, plain steel threads as received. Lubricated: K = 0.15, oiled threads. Plated, waxed or thread-locked threads take a different K and less torque.
  • Torque T = K × D × F, D the nominal diameter, F the clamp load; tensile stress area from ASME B1.1 or ISO 898-1.
  • Steel bolt and nut (or tapped hole) at least as strong as the bolt. Tapped aluminum or cast iron needs less.

Two published copies agree

A starting value, not a spec. Torque is only an indirect measure of clamp load: thread and under-head friction decide how much of it becomes clamp. The joint designer's or equipment maker's torque wins.

Published charts

What published charts print for M18 × 2.5

Dry, on the same basis (75% of proof, K 0.20), in N·m.

Class 8.8
306 N·m (charts print 301–311)Only two makers publish this: Fastenal and AIMS Industrial
Class 10.9
430 N·mOnly two makers publish this: Fastenal and AIMS Industrial
Class 12.9
503 N·mOnly two makers publish this: Fastenal and AIMS Industrial

Only two makers publish this: Fastenal and AIMS Industrial

How it's worked

The arithmetic for Class 10.9

As = .7854 × (18 − .9382 × 2.5)² = 192.5 mm². Class 10.9: F = .75 × 192.5 × 830 MPa = 119,814 N; dry T = .20 × 18 mm × 119,814 N = 431 N·m.

Sources

Sources9