Quoting

Metal weight calculator

Weight and cost of metal plate, bar, tube and angle from its size and alloy.

Weight

10.24lb

Range across the published densities: 10.21 – 10.24 lb

Median of 3 makers

Per foot
10.24 lb/ft
Other unit
4.64 kg
Why these numbers?
  1. Plate / flat bar: A = T × W, with Thickness 0.2500, Width 12.0000 in, gives A = 3.0000 in².
  2. Volume = A × length = 36.000 in³ per piece.
  3. Mild steel (1018) weighs 0.2843 lb/in³: the median of 3 makers (they span 0.2836 lb/in³–0.2843 lb/in³).
  4. Weight = volume × density = 10.24 lb each.

How we source these numbers

Units
Shape

12 ft = 144 in

Your supplier’s price, in any currency

What next

How long per part, and what does it cost?Cycle time from your cuts, feeds and tool changes, then price per part and batch.
What speed and feed for this lathe cut?Lathe SFM, feed and depth of cut for your material and insert, with the RPM.
What feed rate for this end mill?End mill RPM, chip load and feed rate for your material, cutter and cut.
How the metal weight calculator works

A 1/4 in steel plate 12 by 12 in (1018) weighs 10.24 lb (4.64 kg).

How to calculate metal weight

Maintained by John, former CNC lathe programmer

What it does

Weight is cross-section area × length × density. This calculator works out the area for seven stock shapes and multiplies by the length, the number of pieces, and the published density of the alloy you pick. Add your price per pound or kilogram to get the cost of the metal for a quote.

Formulas

Weight

W = A × L × ρ × quantity

A is the cross-section area, L the length, ρ the density (lb/in³ or g/cm³).

Cross-section area by shape
ShapeArea
Plate / flat barA = T × W
Round barA = π × D² ÷ 4
Hex barA = √3 ÷ 2 × F²
Square barA = S²
Round tubeA = π × t × (OD − t)
Square / rectangular tubeA = W × H − (W − 2t)(H − 2t)
AngleA = t × (A + B − t)

Worked example: a 1/2" × 48" × 96" steel plate

  1. A = 0.5 × 48 = 24.0 in²
  2. Volume = 24 × 96 = 2,304 in³
  3. Mild steel (1018) = 0.2843 lb/in³, the median of three published densities
  4. W = 2,304 × 0.2843 = 655.1 lb (297.1 kg)

Metal densities

Each density is checked against every publisher found. Three or more give the median and the span they cover. Two are shown as a range with both named. None of these alloys rests on a single source.

Density of each metal
Metallb/in³g/cm³Sources
Mild steel (1018)0.28430.2836–0.28437.87

Median of 3 makers

Alloy steel (4140)0.28360.2829–0.28367.85

Median of 4 makers

Stainless 3040.28500.2850–0.29007.89

Median of 3 makers

Stainless 3160.29000.2890–0.29018.03

Median of 3 makers

Stainless 17-4 PH0.28180.2818–0.28187.80

Only two makers publish this: AIMS Industrial and Alabama Specialty Products

Aluminum 60610.09750.0975–0.09802.70

Median of 3 makers

Aluminum 70750.10120.1010–0.10152.80

Median of 3 makers

Aluminum 20240.10010.1000–0.10042.77

Median of 3 makers

Brass 360 (C36000)0.30670.3067–0.30718.49

Median of 3 makers

Copper 110 (C11000)0.32120.3212–0.32308.89

Median of 3 makers

Bearing bronze 932 (C93200)0.32190.3219–0.32198.91

Only two makers publish this: Alabama Specialty Products and Austral Wright Metals

Titanium Ti-6Al-4V (grade 5)0.16000.1597–0.16154.43

Median of 4 makers

Gray cast iron0.25510.2518–0.25837.06

Only two makers publish this: AIMS Industrial and Alabama Specialty Products

Tool steel D20.27930.2782–0.28037.73

Only two makers publish this: AIMS Industrial and Alabama Specialty Products

Gotchas

Steel is not one number
Mild steel, 4140 and D2 sit within 2% of each other, 316 stainless is about 2% heavier than mild steel, and bearing bronze about 13% heavier. Pick the alloy, not just "steel".
Hex is across the flats
Measure hex bar flat to flat (the wrench size), not corner to corner; the corners are 15% wider.
Tube corners and angle fillets
The formulas use sharp corners. Formed square tube with rounded corners weighs a little less; rolled angle with a root fillet weighs a little more.
Nominal vs actual size
Pipe is sold by nominal size, and plate and bar run over their nominal thickness. Enter the size you will actually have, and buy to the heavy side of the range.
Cost is metal only
Price × weight is the metal. Cutting, drops, minimum charges and freight come on top.

Sources

The areas are geometry, cited rather than counted. Densities follow the site's tiered source rule; each alloy's publishers and the figure each one prints:

Sheet in gauges: sheet metal gauge chart, with weight per square foot.