ASME B16.5 · Class 150 (150#)

20" Class 150 flange: bolts and torque

A 20" Class 150 flange takes 20 studs, 1-1/8-8 UN, on a 25" bolt circle, 6-1/4" long for a raised face and 6-3/4" for a ring joint. With a spiral wound gasket and B7 studs the gasket makers' tables give 653 ft·lb per stud.

A Class 150 NPS 20 flange face on, to scale: 27-1/2" OD, 20 holes of 1-1/4" on a 25" bolt circle, each with a 1-1/8" stud.OD 27-1/2"bolt circle 25"hole 20 × 1-1/4"bolt 20 × 1-1/8"
The NPS 20 Class 150 flange, face on. To scale.

A starting point from published gasket-maker tables. Your site’s bolting procedure, or a PCC-1 qualified joint procedure, governs pressure piping.

Studs and flange

Studs
20 × 1-1/8-8 UN
Stud length, raised face
6-1/4" (1/16" raised face)
Stud length, ring joint
6-3/4"
Nut wrench
1-13/16" (heavy hex)
Bolt circle
25"
Flange OD
27-1/2"
Bolt holes
1-1/4"

Checked against 3 published copies

Stud lengths are measured first thread to first thread, as B16.5 lists them.

Torque by gasket

Per stud, ASTM A193 B7 studs with 2H nuts, lubricated as each maker's table assumes.

  • Spiral wound653 ft·lb · 885 N·m

    Garlock 710 · Flexitallic 570 · Teadit 595 · FNW 723 ft·lb (span 430–723)

    Median of 4 makers

  • Sheet (PTFE, graphite, fibre)601 ft·lb · 814 N·m

    Garlock 503 · Gore 740 · Thomson 601 ft·lb (span 296–859)

    Median of 3 makers

  • Ring joint (RTJ)645 ft·lb · 874 N·m

    Computed, no maker table: no gasket maker prints ring joint torque per flange size.

    How it's computed

    T = K × D × F at 60% of B7 yield (63 ksi) on the .728 in² root area, K 0.15.

Median of 3 makers

Work it in the calculator: other stud materials (B7M, L7, B8M), your lubricant's K, or your own bolt stress.

Passes (spiral wound, 653 ft·lb)

Passes for the spiral wound gasket, to 653 ft·lb
  1. Snug by hand, then a short wrench, in the star
  2. 30% in the star196 ft·lb
  3. 60–70% in the star392–457 ft·lb
  4. 100% in the star653 ft·lb
  5. Check bolt to bolt round the flange until no nut turns653 ft·lb

The passes as the gasket makers print them.

Tightening order for 20 bolts →

Gaskets for this flange

Spiral wound, sheet and ring joint sizes

Dimensions from ASME B16.20 (spiral wound, ring joint) and B16.21 (sheet), checked against published copies.

Units
Spiral wound
Inner ring ID19.69500.1
Winding ID × OD20.69525.5 × 22.75577.9
Centering ring OD23.88606.4
Inner ringNot required
Sheet ring
ID × OD20.00508.0 × 23.88606.6
Ring joint
Ring numberR-72

Sources

Sources13