ASME B16.21 · non-metallic flat gaskets for ASME B16.5 flanges

Class 150 gasket dimensions

A Class 150 NPS 2 sheet gasket is 2.38" ID × 4.12" OD. Cut sizes for compressed fibre, PTFE, graphite and rubber sheet gaskets. A ring gasket sits inside the bolts on a raised face; a full-face gasket covers a flat-face flange out to its edge, with the bolt holes punched. Each size is checked against three or four published copies of the standard; a tag marks any that differ.

The Class 150 NPS 2 sheet gasket, face on, to scale: size value 2.38" ID × 4.12" OD.2.38" ID × 4.12" OD
The Class 150 NPS 2 sheet gasket, face on. To scale.
Units

Class 150 sheet gasket chart

Class 150 ring and full-face gaskets by pipe size
NPSID (inmm)Ring OD (inmm)Full-face OD (inmm)HolesHole Ø (inmm)Bolt circle (inmm)
1/20.8421.31.8847.83.5088.945/80.6316.02.3860.5
3/41.0626.92.2557.23.8898.645/80.6316.02.7569.9
11.3133.32.6266.54.25108.045/80.6316.03.1379.5
1-1/41.6642.23.0076.24.63117.645/80.6316.03.5088.9
1-1/21.9148.53.3885.95.00127.045/80.6316.03.8898.6
22.3860.54.12104.66.00152.443/40.7519.14.75120.7
2-1/22.8873.24.88124.07.00177.843/40.7519.15.50139.7
33.5088.95.38136.77.50190.543/40.7519.16.00152.4
3-1/24.00101.66.38162.18.50215.983/40.7519.17.00177.8
44.50114.36.88174.89.00228.683/40.7519.17.50190.5
55.56141.27.75196.910.00254.087/80.8822.48.50215.9
66.62168.18.75222.311.00279.487/80.8822.49.50241.3
88.62218.911.00279.413.50342.987/80.8822.411.75298.5
1010.75273.113.38339.916.00406.41211.0025.414.25362.0
1212.75323.916.13409.719.00482.61211.0025.417.00431.8
1414.00355.617.75450.921.00533.4121-1/81.1328.718.75476.3
1616.00406.420.25514.423.50596.9161-1/81.1328.721.25539.8
1818.00457.221.62549.125.00635.0161-1/41.2531.822.75577.9
2020.00508.023.88606.627.50698.5201-1/41.2531.825.00635.0
2424.00609.628.25717.632.00812.8201-3/81.3835.129.50749.3

Per ASME B16.21, checked against Garlock, Lamons and Wermac. B16.21 sets the cut diameters, not the thickness. breakingchips.com/gaskets/sheet/class-150/

Before you cut

The ID, higher classes and full-face sizes
  • The ID is the pipe’s outside diameter (0.84" at NPS 1/2), so it is the same in every class; the OD changes with the bolt circle.
  • B16.21 lists no sheet gaskets above Class 900. For Class 1500 and 2500 use a spiral wound or ring joint gasket.

Sources