ASME B16.5 · Class 1500 (1500#)
Class 1500 flange bolt chart
Class 1500 flanges take 4 studs, 3/4-10 UNC, on a 3-1/4" bolt circle at NPS 1/2, up to 16 studs, 3-1/2-8 UN, on a 39" bolt circle at NPS 24. Studs for every Class 1500 flange, NPS 1/2 to 24: how many, what size, and how long for a raised face (1/4") and a ring joint, with the torque gasket makers publish for B7 studs. Each size has its own page with the pattern and passes.
A starting point from published gasket-maker tables. Your site’s bolting procedure, or a PCC-1 qualified joint procedure, governs pressure piping.
Class 1500 studs and torque
| NPS | Studs | Spiral wound ft·lb | RF length | RTJ length | Bolt circle | Flange OD |
|---|---|---|---|---|---|---|
| 1/2" | 4 × 3/4-10 UNC | 85 | 4-1/4" | 4-1/4" | 3-1/4" | 4-3/4" |
| 3/4" | 4 × 3/4-10 UNC | 100 | 4-1/2" | 4-1/2" | 3-1/2" | 5-1/8" |
| 1" | 4 × 7/8-9 UNC | 160 | 5" | 5" | 4" | 5-7/8" |
| 1-1/4" | 4 × 7/8-9 UNC | 200 | 5" | 5" | 4-3/8" | 6-1/4" |
| 1-1/2" | 4 × 1-8 UNC | 275 | 5-1/2" | 5-1/2" | 4-7/8" | 7" |
| 2" | 8 × 7/8-9 UNC | 200 | 5-3/4" | 5-3/4" | 6-1/2" | 8-1/2" |
| 2-1/2" | 8 × 1-8 UNC | 300 | 6-1/4" | 6-1/4" | 7-1/2" | 9-5/8" |
| 3" | 8 × 1-1/8-8 UN | 400 | 7" | 7" | 8" | 10-1/2" |
| 4" | 8 × 1-1/4-8 UN | 650 | 7-3/4" | 7-3/4" | 9-1/2" | 12-1/4" |
| 5" | 8 × 1-1/2-8 UN | 970 | 9-3/4" | 9-3/4" | 11-1/2" | 14-3/4" |
| 6" | 12 × 1-3/8-8 UN | 867 | 10-1/4" | 10-1/2" | 12-1/2" | 15-1/2" |
| 8" | 12 × 1-5/8-8 UN | 1,297 | 11-1/2" | 12-3/4" | 15-1/2" | 19" |
| 10" | 12 × 1-7/8-8 UN | 2,262 | 13-1/4" | 13-1/2" | 19" | 23" |
| 12" | 16 × 2-8 UN | 2,200 | 14-3/4" | 15-1/4" | 22-1/2" | 26-1/2" |
| 14" | 16 × 2-1/4-8 UN | 3,180 | 16" | 16-3/4" | 25" | 29-1/2" |
| 16" | 16 × 2-1/2-8 UN | 4,400 | 17-1/2" | 18-1/2" | 27-3/4" | 32-1/2" |
| 18" | 16 × 2-3/4-8 UN | 5,920 | 19-1/2" | 20-3/4" | 30-1/2" | 36" |
| 20" | 16 × 3-8 UN | 7,720 | 21-1/4" | 22-1/4" | 32-3/4" | 38-3/4" |
| 24" | 16 × 3-1/2-8 UN | 12,750 | 24-1/4" | 25-1/2" | 39" | 46" |
Torque is per stud: the median of the gasket makers' tables, or * where only two makers publish that size (both are named on its page). — means fewer than two publish it, and sheet gaskets are refused above Class 300 (the makers say to ask them). Ring joint torque is computed on each size's page.
Checked against 5 published copies
Where the copies differ, the row shows what most print: NPS 8 RTJ length (Texas Flange and Wermac 11-3/4"; DNOW and Lamons 12-3/4").
Sources
Sources6
- ASME B16.5 — Pipe flanges and flanged fittings, NPS 1/2 through NPS 24
- Lamons — Gasket Handbook 2023: bolt reference charts for ASME B16.5 flanges (archived Aug 12, 2025)
- Engineering ToolBox — ASME/ANSI B16.5 flanges and bolt dimensions, Class 150 to 2500 (archived Oct 11, 2026)
- Wermac — Weld neck flanges and stud bolts, ASME B16.5, dimensions in inches (per class) (archived Jun 19, 2025)
- Texas Flange — Bolt and stud dimensions for ASME B16.5 flanges (archived Sep 23, 2026)
- DistributionNOW — Number and size of bolts for flanged joints, ASME B16.5 (archived Jun 19, 2025)
- Gasket makers' torque tables: named on each size's page.