ASME B16.5 · Class 1500 (1500#)

14" Class 1500 flange: bolts and torque

A 14" Class 1500 flange takes 16 studs, 2-1/4-8 UN, on a 25" bolt circle, 16" long for a raised face and 16-3/4" for a ring joint. With a spiral wound gasket and B7 studs the gasket makers' tables give 3,180 ft·lb per stud.

A Class 1500 NPS 14 flange face on, to scale: 29-1/2" OD, 16 holes of 2-3/8" on a 25" bolt circle, each with a 2-1/4" stud.OD 29-1/2"bolt circle 25"hole 16 × 2-3/8"bolt 16 × 2-1/4"
The NPS 14 Class 1500 flange, face on. To scale.

A starting point from published gasket-maker tables. Your site’s bolting procedure, or a PCC-1 qualified joint procedure, governs pressure piping.

Studs and flange

Studs
16 × 2-1/4-8 UN
Stud length, raised face
16" (1/4" raised face)
Stud length, ring joint
16-3/4"
Nut wrench
3-1/2" (heavy hex)
Bolt circle
25"
Flange OD
29-1/2"
Bolt holes
2-3/8"

Checked against 3 published copies

Stud lengths are measured first thread to first thread, as B16.5 lists them.

Torque by gasket

Per stud, ASTM A193 B7 studs with 2H nuts, lubricated as each maker's table assumes.

  • Spiral wound3,180 ft·lb · 4,312 N·m

    Garlock 3,180 · Flexitallic 2,650 · Teadit 3,200 ft·lb (span 684–3,200)

    Median of 3 makers

  • Sheet (PTFE, graphite, fibre)

    Not shown: Sheet gasket makers publish torque only for Class 150 and 300 flanges; above that they say to ask them.

  • Ring joint (RTJ)6,065 ft·lb · 8,223 N·m

    Computed, no maker table: no gasket maker prints ring joint torque per flange size.

    How it's computed

    T = K × D × F at 60% of B7 yield (63 ksi) on the 3.423 in² root area, K 0.15.

Median of 3 makers

Work it in the calculator: other stud materials (B7M, L7, B8M), your lubricant's K, or your own bolt stress.

Passes (spiral wound, 3,180 ft·lb)

Passes for the spiral wound gasket, to 3,180 ft·lb
  1. Snug by hand, then a short wrench, in the star
  2. 30% in the star954 ft·lb
  3. 60–70% in the star1,908–2,226 ft·lb
  4. 100% in the star3,180 ft·lb
  5. Check bolt to bolt round the flange until no nut turns3,180 ft·lb

The passes as the gasket makers print them.

Tightening order for 16 bolts →

Gaskets for this flange

Spiral wound, sheet and ring joint sizes

Dimensions from ASME B16.20 (spiral wound, ring joint) and B16.21 (sheet), checked against published copies.

Units
Spiral wound
Inner ring ID12.63320.8
Winding ID × OD14.25362.0 × 15.75400.1
Centering ring OD22.75577.9
Inner ringRequired
Sheet ring
ASME B16.21 lists no sheet gaskets above Class 900; only Garlock prints these sizes, and it says to consult it
Ring joint
Ring numberR-63

Sources

Sources9