Ring joint gasket · ASME B16.20 type R

R-62 ring gasket dimensions

R-62 is a ring joint (RTJ) gasket with a 16.500" pitch diameter and a 0.625" wide ring, made oval or octagonal. It fits NPS 14 Class 900 flanges.

R-62 ring joint gasket, its oval and octagonal cross sections to one scale, with the width A, heights B and H, and flat C.A 0.625"B 0.88"C 0.413"H 0.81"ovaloctagonal
R-62, 16.500" pitch diameter: its two cross sections. Both sections to one scale.
Units

Pitch diameter P

16.500419.10inmm

Width A

0.62515.88inmm

Height, oval B

0.8822.4inmm

Height, octagonal H

0.8120.6inmm

Flat width C (octagonal)

0.41310.49inmm

Flanges it fits

ASME B16.5 ring type joint flanges that take R-62, by the published copies of the ring-number table.

Oval or octagonal

Both shapes, one groove: which to order

R-62 is made in both shapes on the same pitch diameter and width; only the height differs. Either seals in the flat-bottomed groove of a current flange, and only the oval fits an old round-bottomed groove (Lamons, Flexitallic). Order it by number, shape and material, e.g. "R-62 octagonal, soft iron". Flexitallic recommends a new ring each time the joint is opened.

Sources

Sources4