Class 900 spiral wound gasket dimensions
A Class 900 NPS 3 spiral wound gasket winds from 3.75" to 4.75" on a 6.63" centering ring. The four diameters of a spiral wound gasket with inner and centering rings, NPS 1/2 to 24. Each is checked against three published copies of the standard (two for the inner ring); a tag marks any size where they differ.
Class 900 spiral wound gasket chart
| NPS | Inner ring ID (inmm) | Winding ID (inmm) | Winding OD (inmm) | Centering ring OD (inmm) | Inner ring |
|---|---|---|---|---|---|
| 1/2 | B16.5 has no Class 900 flange below NPS 3: use the Class 1500 gasket | ||||
| 3/4 | B16.5 has no Class 900 flange below NPS 3: use the Class 1500 gasket | ||||
| 1 | B16.5 has no Class 900 flange below NPS 3: use the Class 1500 gasket | ||||
| 1-1/4 | B16.5 has no Class 900 flange below NPS 3: use the Class 1500 gasket | ||||
| 1-1/2 | B16.5 has no Class 900 flange below NPS 3: use the Class 1500 gasket | ||||
| 2 | B16.5 has no Class 900 flange below NPS 3: use the Class 1500 gasket | ||||
| 2-1/2 | B16.5 has no Class 900 flange below NPS 3: use the Class 1500 gasket | ||||
| 3 | 3.1078.7 | 3.7595.3 | 4.75120.7 | 6.63168.3 | Not required |
| 4 | 4.04102.6 | 4.75120.7 | 5.88149.2 | 8.13206.4 | Not required |
| 5 | 5.05128.3 | 5.81147.6 | 7.00177.8 | 9.75247.7 | Not required |
| 6 | 6.10154.9 | 6.88174.6 | 8.25209.6 | 11.38288.9 | Not required |
| 8 | 7.75196.9 | 8.75222.3 | 10.13257.2 | 14.13358.8 | Not required |
| 10 | 9.69246.1 | 10.88276.2 | 12.25311.2 | 17.13435.0 | Not required |
| 12 | 11.50292.1 | 12.75323.9 | 14.50368.3 | 19.63498.5 | Not required |
| 14 | 12.63320.8 | 14.00355.6 | 15.75400.1 | 20.50520.7 | Not required |
| 16 | 14.75374.7 | 16.25412.8 | 18.00457.2 | 22.63574.7 | Not required |
| 18 | 16.75425.5 | 18.25463.6 | 20.50520.7 | 25.13638.2 | Not required |
| 20 | 19.00482.6 | 20.50520.7 | 22.50571.5 | 27.50698.5 | Not required |
| 24 | 23.25590.6 | 24.75628.7 | 26.75679.5 | 33.00838.2 | Required |
Per ASME B16.20, checked against Lamons, Flexitallic and APG. Winding 0.175" (4.45 mm) thick; rings 0.117–0.131". breakingchips.com/gaskets/spiral-wound/class-900/
Thickness
Show
- Winding
- 0.175" (4.45 mm), uncompressed
- Inner and centering rings
- 0.117–0.131" (2.97–3.33 mm), nominally 1/8"
The rings stop the winding crushing: the joint is made up when the flanges close on them. Winding: Flexitallic and Wermac; ring range: Lamons and Wermac.
When the inner ring is required
Show
- Class 900 NPS 24, Class 1500 NPS 12–24 and Class 2500 NPS 4–12 (on this chart: NPS 24).
- Any PTFE-filled winding, at every size.
- Flexitallic also fits one to every flexible graphite gasket unless the buyer says not to.
Elsewhere it is optional, though many makers fit one by default: it keeps the winding from buckling inward and smooths the flow past the joint. Lamons, Flexitallic and APG all print these rules.
Other Class 900 gaskets
Sources
Sources5
The standard is ASME B16.20 — Metallic Gaskets for Pipe Flanges (ring joint, spiral wound and jacketed) (archived Jul 10, 2026). Its sizes are checked against these copies, not averaged: a value is the one the copies print (Flexitallic prints fractions, so 1-7/8" is shown as 1.88" and 47.6 mm). Millimetres are inches × 25.4.
- Lamons — Gasket Handbook 2023: B16.21 ring and full-face gaskets (pp. 39–42), spiral wound WRI to B16.20 (pp. 72–77), ring joint (pp. 117–119) (archived Aug 12, 2025)
- Flexitallic — Spiral Wound Gaskets catalog: Style CG & CGI to ASME B16.20, Tables 1 and 3 (pp. 8–10) (archived Feb 5, 2023)
- APG (callapg.com) — ASME B16.20 spiral wound gasket dimensions for B16.5 flanges (catalog p. 14)
- Wermac — Dimensions of spiral wound gaskets, ASME B16.20 (thickness of rings and sealing element) (archived Nov 14, 2025)