ASTM E140 · Non-austenitic steel

51 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 51 HRC equals 528 HV (Vickers) and 496 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

51 HRC on the three scales: 496 HB and 528 HV, as ASTM E140 converts it.HRCHBHVHRC 51HB 496HV 52820253035404565300400700300400600700900
51 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
496 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
528 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 48 to 54 in Vickers and Brinell
HRCHVHB
48 HRC484455
49 HRC498469
50 HRC513481
51 HRC528496
52 HRC544512
53 HRC560525
54 HRC577543

Sources

Sources5