ASTM E140 · Non-austenitic steel

49 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 49 HRC equals 498 HV (Vickers) and 469 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

49 HRC on the three scales: 469 HB and 498 HV, as ASTM E140 converts it.HRCHBHVHRC 49HB 469HV 4982025303540456065300400700300400600700900
49 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
469 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
498 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 46 to 52 in Vickers and Brinell
HRCHVHB
46 HRC458432
47 HRC471443
48 HRC484455
49 HRC498469
50 HRC513481
51 HRC528496
52 HRC544512

Sources