ASTM E140 · Non-austenitic steel

56 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 56 HRC equals 613 HV (Vickers) and 577 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

56 HRC on the three scales: 577 HB and 613 HV, as ASTM E140 converts it.HRCHBHVHRC 56HB 577HV 6132025303540456065300400700300400500700900
56 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
577 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
613 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 53 to 59 in Vickers and Brinell
HRCHVHB
53 HRC560525
54 HRC577543
55 HRC595560
56 HRC613577
57 HRC633595
58 HRC653615
59 HRC674634

Sources

Sources5