ASTM E140 · Non-austenitic steel

59 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 59 HRC equals 674 HV (Vickers) and 634 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

59 HRC on the three scales: 634 HB and 674 HV, as ASTM E140 converts it.HRCHBHVHRC 59HB 634HV 67420253035404565300400700300400500600900
59 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
634 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
674 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 56 to 62 in Vickers and Brinell
HRCHVHB
56 HRC613577
57 HRC633595
58 HRC653615
59 HRC674634
60 HRC697(654)
61 HRC720(670)
62 HRC746(688)

Sources

Sources5