ASTM E140 · Non-austenitic steel
68 HRC to HV (ASTM E140)
By ASTM E140 Table 1, 68 HRC equals 940 HV (Vickers); E140 gives no Brinell above HRC 65. For carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.
- Brinell
- None: E140 gives no Brinell above HRC 65.
- Vickers
- 940 HV
Checked against 5 published copies
Nearby values
Sources
Sources5
ASTM E140, Standard Hardness Conversion Tables for Metals, Tables 1 and 2 (non-austenitic steels). Every value on this page was checked against these published copies:
- Phase II — Rockwell C hardness conversion chart (ASTM E140 Table 1) (archived May 13, 2026)
- LabTesting — Rockwell C hardness conversion, non-austenitic steels (archived Jul 13, 2026)
- NSM — Hardness conversion calculator (ASTM E140 Tables 1 and 2) (archived Nov 16, 2026)
- Misumi — Conversion table of hardness, SAE J417 (from ASTM E140 Table 1) (archived Nov 15, 2026)
- Honesdom (hardnessgauge.com) — Hardness conversion chart, Rockwell C (archived May 15, 2026)