ASTM E140 · Non-austenitic steel

66 HRC to HV (ASTM E140)

By ASTM E140 Table 1, 66 HRC equals 865 HV (Vickers); E140 gives no Brinell above HRC 65. For carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

66 HRC on the three scales: no Brinell (E140 gives none above HRC 65) and 865 HV, as ASTM E140 converts it.HRCHBHVHRC 66HV 865202530354045505560300400500300400500600700
66 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
None: E140 gives no Brinell above HRC 65.
Vickers
865 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 63 to 68 in Vickers and Brinell
HRCHVHB
63 HRC772(705)
64 HRC800(722)
65 HRC832(739)
66 HRC865—
67 HRC900—
68 HRC940—

Sources

Sources5