Heli-Coil insert · 1/2-20 UNF
1/2-20 Helicoil drill size
The Heli-Coil drill for 1/2-20 is 33/64" (0.5156", 13.10 mm) in aluminum and steel. Countersink 120°, then tap with the 1/2-20 STI tap, not the standard 1/2-20 tap: the insert's wire needs a hole 0.0650" bigger on every diameter.
Aluminum
33/64
0.5156" · 13.10 mm
Steel, magnesium, plastic
33/64
0.5156" · 13.10 mm
One source: Heli-Coil, the insert’s maker (HC-2000)
1/2-20 STI thread (tapped hole, minimum)
- Major Ø
- 0.565" (14.35 mm)
- Pitch Ø
- 0.532" (13.52 mm)
- Minor Ø
- 0.511" (12.97 mm)
- Threads per inch
- 20
How these are worked
Each is the 1/2-20 UNF basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.
Two published copies agree
Minimum tapping depth
Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.
| Insert | Insert length | Tap at least |
|---|---|---|
| 1 × D | 0.500" | 0.550" |
| 1.5 × D | 0.750" | 0.800" |
| 2 × D | 1.000" | 1.050" |
| 2.5 × D | 1.250" | 1.300" |
| 3 × D | 1.500" | 1.550" |
One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)
Sources
Sources3
- Stanley Engineered Fastening — Heli-Coil inserts, HC-2000 rev 11: Tables V–VIII, drilled and tapped hole dimensions (archived Nov 25, 2024)
- Amesweb — Helicoil tap sizes (STI), after ASME B18.29.1 (archived Jul 11, 2026)
- ASME B18.29.1 — Helical coil screw thread inserts, free running and screw locking (inch series)