Heli-Coil insert · 7/16-20 UNF
7/16-20 Helicoil drill size
The Heli-Coil drill for 7/16-20 is 29/64" (0.4531", 11.51 mm) in aluminum and steel. Countersink 120°, then tap with the 7/16-20 STI tap, not the standard 7/16-20 tap: the insert's wire needs a hole 0.0650" bigger on every diameter.
Aluminum
29/64
0.4531" · 11.51 mm
Steel, magnesium, plastic
29/64
0.4531" · 11.51 mm
One source: Heli-Coil, the insert’s maker (HC-2000)
7/16-20 STI thread (tapped hole, minimum)
- Major Ø
- 0.502" (12.76 mm)
- Pitch Ø
- 0.470" (11.94 mm)
- Minor Ø
- 0.448" (11.39 mm)
- Threads per inch
- 20
How these are worked
Each is the 7/16-20 UNF basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.
Two published copies agree
Minimum tapping depth
Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.
| Insert | Insert length | Tap at least |
|---|---|---|
| 1 × D | 0.438" | 0.488" |
| 1.5 × D | 0.656" | 0.706" |
| 2 × D | 0.875" | 0.925" |
| 2.5 × D | 1.094" | 1.144" |
| 3 × D | 1.313" | 1.363" |
One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)
Sources
Sources3
- Stanley Engineered Fastening — Heli-Coil inserts, HC-2000 rev 11: Tables V–VIII, drilled and tapped hole dimensions (archived Nov 25, 2024)
- Amesweb — Helicoil tap sizes (STI), after ASME B18.29.1 (archived Jul 11, 2026)
- ASME B18.29.1 — Helical coil screw thread inserts, free running and screw locking (inch series)