Sheet metal gauge
23 gauge sheet metal thickness
23 gauge sheet metal is 0.0269" (0.68 mm) in steel, 0.0306" (0.78 mm) galvanized, 0.0281" (0.71 mm) stainless and 0.0226" (0.57 mm) aluminum. Each metal has its own gauge system, and gauge is nominal: measure the stock when the thickness matters.
Steel
0.0269"
0.68 mm
Manufacturers' Standard Gauge
Galvanized steel
0.0306"
0.78 mm
Galvanized Sheet Gauge
Stainless steel
0.0281"
0.71 mm
U.S. Standard Gauge
Aluminum
0.0226"
0.57 mm
Brown & Sharpe (AWG)
Two published copies agree
Weight
| Material | lb/ft² | kg/m² |
|---|---|---|
| Steel | 1.125 | 5.49 |
| Galvanized steel | 1.281 | 6.26 |
| Stainless steel | 1.154 | 5.64 |
| Aluminum | 0.317 | 1.55 |
From the standard, Manufacturers' Standard Gauge
How each weight is worked
- Steel: Defined by weight: the U.S. Standard Gauge weight per square foot.
- Galvanized steel: Defined by weight: the U.S. Standard Gauge weight plus 2.5 oz/ft² of zinc.
- Stainless steel: For 304 at 0.285 lb/in³ (datasheets span 0.285–0.290).
- Aluminum: For 6061 at 0.0975 lb/in³ (datasheets span 0.0975–0.0980).
Sources
Sources12
- 15 U.S.C. § 206, Standard gauge for sheet and plate iron and steel (the weights) (archived Oct 13, 2026)
- Continental Steel, Galvanized sheets: each gauge is 2.5 oz/ft² heavier than the U.S. Standard Gauge (archived Nov 15, 2026)
- 15 U.S.C. § 206, Standard gauge for sheet and plate iron and steel (archived Oct 13, 2026)
- Math: American Wire Gauge (ASTM B258) is defined by 0.005" × 92^((36 − n) / 39), exact by definition (cited, not counted)
- Wikipedia, Sheet metal: gauge table (steel column from Machinery's Handbook, 27th ed.) (archived Oct 21, 2026)
- American Steel & Aluminum, Sheet metal gauge chart (archived Nov 13, 2026)
- Cleveland-Cliffs, 304/304L stainless product data bulletin (archived Nov 15, 2026)
- Rolled Alloys, 304/304L stainless steel data sheet (archived May 13, 2025)
- Outokumpu, 304/304L data sheet (Imperial, Americas) (archived Nov 2, 2026)
- Protolabs, Aluminum 6061-T651/T6 material data sheet
- Smiths Advanced Metals, 6061 aluminium sheet (archived Nov 16, 2026)
- Alabama Specialty Products, alloy density table (A96061 Al 6061) (archived Oct 14, 2026)