Sheet metal gauge

27 gauge sheet metal thickness

27 gauge sheet metal is 0.0164" (0.42 mm) in steel, 0.0202" (0.51 mm) galvanized, 0.0172" (0.44 mm) stainless and 0.0142" (0.36 mm) aluminum. Each metal has its own gauge system, and gauge is nominal: measure the stock when the thickness matters.

Steel

0.0164"

0.42 mm

Manufacturers' Standard Gauge

Galvanized steel

0.0202"

0.51 mm

Galvanized Sheet Gauge

Stainless steel

0.0172"

0.44 mm

U.S. Standard Gauge

Aluminum

0.0142"

0.36 mm

Brown & Sharpe (AWG)

From the standard, U.S. Standard Gauge

Weight

27 gauge sheet weight by material
Materiallb/ft²kg/m²
Steel0.6883.36
Galvanized steel0.8444.12
Stainless steel0.7053.44
Aluminum0.1990.97

From the standard, Manufacturers' Standard Gauge

How each weight is worked
  • Steel: Defined by weight: the U.S. Standard Gauge weight per square foot.
  • Galvanized steel: Defined by weight: the U.S. Standard Gauge weight plus 2.5 oz/ft² of zinc.
  • Stainless steel: For 304 at 0.285 lb/in³ (datasheets span 0.285–0.290).
  • Aluminum: For 6061 at 0.0975 lb/in³ (datasheets span 0.0975–0.0980).

Sources