Lathe threading · 60° thread

0.5 mm pitch threading: depth and passes

Single-point a 0.5 mm pitch thread in 4 passes: 0.307 mm deep outside (0.352 mm on a compound at 29.5°), 0.271 mm inside. First pass 0.097 mm, last 0.056 mm. Fanuc G76, external: P307 Q97.

Outside (shaft)

0.307 mm

4 passes

Inside (bore)

0.271 mm

3 passes

Median of 3 makers

External thread (on a shaft): each of the 4 passes
0.5 mm pitch external thread: each pass
PassCut (radial)Total depthCompound at 29.5°
10.097 mm0.097 mm0.111 mm
20.080 mm0.177 mm0.203 mm
30.073 mm0.250 mm0.288 mm
40.056 mm0.307 mm0.352 mm
Internal thread (in a bore): each of the 3 passes
0.5 mm pitch internal thread: each pass
PassCut (radial)Total depthCompound at 29.5°
10.105 mm0.105 mm0.120 mm
20.087 mm0.191 mm0.220 mm
30.079 mm0.271 mm0.311 mm

G76 numbers (Fanuc two-line)

External: thread height P307, first cut Q97. Internal: P271,Q105. In µm, written with no decimal point. The control shrinks each pass after the first the same way as the table.

The whole G76 block, Fanuc or Haas, for your thread

Why each pass cuts less

The √x rule, and the smallest pass

A threading tool cuts on a V, so as it goes deeper more of its edge is in the cut. Taking the same depth every pass would load the last passes far harder than the first. Sandvik’s rule, used here, makes the total depth after pass x grow with √x, so every pass removes about the same area of chip. Passes are the makers’ counts for this pitch, and none is under 0.05 mm (Kennametal), or the tool rubs instead of cutting.

Sources

Sources5