Lathe threading · 60° thread

1.25 mm pitch threading: depth and passes

Single-point a 1.25 mm pitch thread in 7 passes: 0.767 mm deep outside (0.881 mm on a compound at 29.5°), 0.677 mm inside. First pass 0.171 mm, last 0.067 mm. Fanuc G76, external: P767 Q171.

Outside (shaft)

0.767 mm

7 passes

Inside (bore)

0.677 mm

7 passes

Median of 3 makers

External thread (on a shaft): each of the 7 passes
1.25 mm pitch external thread: each pass
PassCut (radial)Total depthCompound at 29.5°
10.171 mm0.171 mm0.197 mm
20.142 mm0.313 mm0.360 mm
30.130 mm0.443 mm0.509 mm
40.099 mm0.542 mm0.623 mm
50.084 mm0.626 mm0.719 mm
60.074 mm0.700 mm0.804 mm
70.067 mm0.767 mm0.881 mm
Internal thread (in a bore): each of the 7 passes
1.25 mm pitch internal thread: each pass
PassCut (radial)Total depthCompound at 29.5°
10.151 mm0.151 mm0.174 mm
20.125 mm0.276 mm0.317 mm
30.114 mm0.391 mm0.449 mm
40.088 mm0.478 mm0.550 mm
50.074 mm0.552 mm0.635 mm
60.065 mm0.618 mm0.710 mm
70.059 mm0.677 mm0.777 mm

G76 numbers (Fanuc two-line)

External: thread height P767, first cut Q171. Internal: P677,Q151. In µm, written with no decimal point. The control shrinks each pass after the first the same way as the table.

The whole G76 block, Fanuc or Haas, for your thread

Why each pass cuts less

The √x rule, and the smallest pass

A threading tool cuts on a V, so as it goes deeper more of its edge is in the cut. Taking the same depth every pass would load the last passes far harder than the first. Sandvik’s rule, used here, makes the total depth after pass x grow with √x, so every pass removes about the same area of chip. Passes are the makers’ counts for this pitch, and none is under 0.05 mm (Kennametal), or the tool rubs instead of cutting.

Sources

Sources5