e8 tolerance for shafts over 0 up to 3 mm is −0.014 / −0.028 mm (−0.00055 / −0.00110 in). A 3 mm e8 shaft measures 2.972–2.986 mm; a 2 mm one, 1.972–1.986 mm. The table gives each common size in the range in mm and inches.

e8 shaft tolerance zone, 0–3 mm: es −14 µm, ei −28 µm against the zero line.es −14 µmei −28 µmtolerance zone e8zero line 0–3 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

e8 limits, over 0 up to 3 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

e8 deviations over 0 up to 3 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
0–3−14−28−0.014−0.028−0.00055−0.0011014

Checked against 3 published copies

Common sizes, e8 shaft

The smallest and largest shaft each size allows.

e8 smallest and largest size for common sizes over 0 up to 3 mm
SizeMin mmMax mmSize inMin inMax in
1 e80.9720.9860.03940.038270.03882
1.5 e81.4721.4860.05910.057950.05850
2 e81.9721.9860.07870.077640.07819
2.5 e82.4722.4860.09840.097320.09787
3 e82.9722.9860.11810.117010.11756