ISO 286 · Shaft · 3–6 mm

e8 shaft tolerance, 3–6 mm

e8 tolerance for shafts over 3 up to 6 mm is −0.020 / −0.038 mm (−0.00079 / −0.00150 in). A 6 mm e8 shaft measures 5.962–5.980 mm; a 5 mm one, 4.962–4.980 mm. The table gives each common size in the range in mm and inches.

e8 shaft tolerance zone, 3–6 mm: es −20 µm, ei −38 µm against the zero line.es −20 µmei −38 µmtolerance zone e8zero line 3–6 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

e8 limits, over 3 up to 6 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

e8 deviations over 3 up to 6 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
3–6−20−38−0.020−0.038−0.00079−0.0015018

Checked against 4 published copies

Common sizes, e8 shaft

The smallest and largest shaft each size allows. 3 mm itself belongs to the range below.

e8 smallest and largest size for common sizes over 3 up to 6 mm
SizeMin mmMax mmSize inMin inMax in
4 e83.9623.9800.15750.155980.15669
5 e84.9624.9800.19690.195350.19606
6 e85.9625.9800.23620.234720.23543

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4