ISO 286 · Shaft · 315–400 mm

g6 shaft tolerance, 315–400 mm

g6 tolerance for shafts over 315 up to 400 mm is −0.018 / −0.054 mm (−0.00071 / −0.00213 in). A 400 mm g6 shaft measures 399.946–399.982 mm; a 350 mm one, 349.946–349.982 mm. The table gives each common size in the range in mm and inches.

g6 shaft tolerance zone, 315–400 mm: es −18 µm, ei −54 µm against the zero line.es −18 µmei −54 µmtolerance zone g6zero line 315–400 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

g6 limits, over 315 up to 400 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

g6 deviations over 315 up to 400 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
315–400−18−54−0.018−0.054−0.00071−0.0021336

Checked against 4 published copies

Common sizes, g6 shaft

The smallest and largest shaft each size allows. 315 mm itself belongs to the range below.

g6 smallest and largest size for common sizes over 315 up to 400 mm
SizeMin mmMax mmSize inMin inMax in
320 g6319.946319.98212.598412.5963012.59772
350 g6349.946349.98213.779513.7774013.77882
400 g6399.946399.98215.748015.7459115.74732

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4