g7 shaft tolerance, 315–400 mm
g7 tolerance for shafts over 315 up to 400 mm is −0.018 / −0.075 mm (−0.00071 / −0.00295 in). A 400 mm g7 shaft measures 399.925–399.982 mm; a 350 mm one, 349.925–349.982 mm. The table gives each common size in the range in mm and inches.
g7 limits, over 315 up to 400 mm
Deviations from the nominal size. Inches are the µm values ÷ 25,400.
| Size, mm | Upper µm | Lower µm | Upper mm | Lower mm | Upper in | Lower in | Band µm |
|---|---|---|---|---|---|---|---|
| 315–400 | −18 | −75 | −0.018 | −0.075 | −0.00071 | −0.00295 | 57 |
Checked against 3 published copies
Common sizes, g7 shaft
The smallest and largest shaft each size allows. 315 mm itself belongs to the range below.
| Size | Min mm | Max mm | Size in | Min in | Max in |
|---|---|---|---|---|---|
| 320 g7 | 319.925 | 319.982 | 12.5984 | 12.59547 | 12.59772 |
| 350 g7 | 349.925 | 349.982 | 13.7795 | 13.77657 | 13.77882 |
| 400 g7 | 399.925 | 399.982 | 15.7480 | 15.74508 | 15.74732 |
Checked against 3 published copies
ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.
Sources
Sources3