ISO 286 · Shaft

g7 shaft tolerance

g7 tolerance on a 25 mm shaft is −0.007 / −0.028 mm, so the shaft measures 24.972–24.993 mm. A g shaft sits wholly below the nominal size, so it clears an H hole. Grade 7 (IT7) sets the band’s width; the chart below gives it for every size to 500 mm.

G7 hole on 25 mm: +0.028 / +0.007 mm. G7 hole tolerance

g7 shaft tolerance zone for every size range from 0–3 mm to 400–500 mm, against the zero line; 18–30 mm is −7 / −28 µm.tolerance zone g7, 18–30 mm: −7 / −28 µmsize range 0–3 to 400–500 mm
One band per size range against the zero line. The marked band holds 25 mm. Deviations to scale; the size ranges are evenly spaced, not to scale.

Limits by size

Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.

g7 limits by nominal size
Size, mmUpper µmLower µmUpper inLower in
0–3−2−12−0.00008−0.00047
3–6−4−16−0.00016−0.00063
6–10−5−20−0.00020−0.00079
10–18−6−24−0.00024−0.00094
18–30−7−28−0.00028−0.00110
30–50−9−34−0.00035−0.00134
50–80−10−40−0.00039−0.00157
80–120−12−47−0.00047−0.00185
120–180−14−54−0.00055−0.00213
180–250−15−61−0.00059−0.00240
250–315−17−69−0.00067−0.00272
315–400−18−75−0.00071−0.00295
400–500−20−83−0.00079−0.00327

Checked against 3 published copies

Any size and fit in the calculator

Sources

Sources3