ISO 286 · Hole
N6 hole tolerance
N6 tolerance on a 25 mm hole is −0.011 / −0.024 mm, so the hole measures 24.976–24.989 mm. An N hole sits at or below the nominal size, for transition and interference fits on an h shaft. Grade 6 (IT6) sets the band’s width; the chart below gives it for every size to 500 mm.
n6 shaft on 25 mm: +0.028 / +0.015 mm. n6 shaft tolerance
Limits by size
Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.
| Size, mm | Upper µm | Lower µm | Upper in | Lower in |
|---|---|---|---|---|
| 0–3 | −4 | −10 | −0.00016 | −0.00039 |
| 3–6 | −5 | −13 | −0.00020 | −0.00051 |
| 6–10 | −7 | −16 | −0.00028 | −0.00063 |
| 10–18 | −9 | −20 | −0.00035 | −0.00079 |
| 18–30 | −11 | −24 | −0.00043 | −0.00094 |
| 30–50 | −12 | −28 | −0.00047 | −0.00110 |
| 50–80 | −14 | −33 | −0.00055 | −0.00130 |
| 80–120 | −16 | −38 | −0.00063 | −0.00150 |
| 120–180 | −20 | −45 | −0.00079 | −0.00177 |
| 180–250 | −22 | −51 | −0.00087 | −0.00201 |
| 250–315 | −25 | −57 | −0.00098 | −0.00224 |
| 315–400 | −26 | −62 | −0.00102 | −0.00244 |
| 400–500 | −27 | −67 | −0.00106 | −0.00264 |
Checked against 4 published copies
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)