ISO 286 · Hole
N7 hole tolerance
N7 tolerance on a 25 mm hole is −0.007 / −0.028 mm, so the hole measures 24.972–24.993 mm. An N hole sits at or below the nominal size, for transition and interference fits on an h shaft. Grade 7 (IT7) sets the band’s width; the chart below gives it for every size to 500 mm.
n7 shaft on 25 mm: +0.036 / +0.015 mm. n7 shaft tolerance
Limits by size
Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.
| Size, mm | Upper µm | Lower µm | Upper in | Lower in |
|---|---|---|---|---|
| 0–3 | −4 | −14 | −0.00016 | −0.00055 |
| 3–6 | −4 | −16 | −0.00016 | −0.00063 |
| 6–10 | −4 | −19 | −0.00016 | −0.00075 |
| 10–18 | −5 | −23 | −0.00020 | −0.00091 |
| 18–30 | −7 | −28 | −0.00028 | −0.00110 |
| 30–50 | −8 | −33 | −0.00031 | −0.00130 |
| 50–80 | −9 | −39 | −0.00035 | −0.00154 |
| 80–120 | −10 | −45 | −0.00039 | −0.00177 |
| 120–180 | −12 | −52 | −0.00047 | −0.00205 |
| 180–250 | −14 | −60 | −0.00055 | −0.00236 |
| 250–315 | −14 | −66 | −0.00055 | −0.00260 |
| 315–400 | −16 | −73 | −0.00063 | −0.00287 |
| 400–500 | −17 | −80 | −0.00067 | −0.00315 |
Checked against 4 published copies
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)