ISO 286 · Shaft · 120–180 mm
p6 shaft tolerance, 120–180 mm
p6 tolerance for shafts over 120 up to 180 mm is +0.068 / +0.043 mm (+0.00268 / +0.00169 in). A 150 mm p6 shaft measures 150.043–150.068 mm; a 160 mm one, 160.043–160.068 mm. The table gives each common size in the range in mm and inches.
p6 limits, over 120 up to 180 mm
Deviations from the nominal size. Inches are the µm values ÷ 25,400.
| Size, mm | Upper µm | Lower µm | Upper mm | Lower mm | Upper in | Lower in | Band µm |
|---|---|---|---|---|---|---|---|
| 120–180 | +68 | +43 | +0.068 | +0.043 | +0.00268 | +0.00169 | 25 |
Checked against 4 published copies
Common sizes, p6 shaft
The smallest and largest shaft each size allows. 120 mm itself belongs to the range below.
| Size | Min mm | Max mm | Size in | Min in | Max in |
|---|---|---|---|---|---|
| 130 p6 | 130.043 | 130.068 | 5.1181 | 5.11980 | 5.12079 |
| 140 p6 | 140.043 | 140.068 | 5.5118 | 5.51350 | 5.51449 |
| 150 p6 | 150.043 | 150.068 | 5.9055 | 5.90720 | 5.90819 |
| 160 p6 | 160.043 | 160.068 | 6.2992 | 6.30091 | 6.30189 |
| 180 p6 | 180.043 | 180.068 | 7.0866 | 7.08831 | 7.08929 |
Checked against 4 published copies
ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page comes from the same engine as the p6 chart, checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)