Burrs where the drill breaks through
Mitsubishi says: use a drill with a smaller edge hone; lower the feed as the drill breaks through.
What you see
A ragged lip of metal around the hole where the drill comes out.
Causes and what to change
Every fix here is from Mitsubishi's troubleshooting guide, unless marked. Change one thing at a time.
An edge hone too large
Use a drill with a smaller edge hone
Feed too high as the drill breaks through
Lower the feed as the drill breaks through
Work it out: Drilling speeds and feeds calculator
Work it out
Often comes with