Rough or torn hole walls
OSG says: regrind until all the wear is gone; change how coolant reaches the point, and raise its volume; check runout at the holder, or use another holder, and check again once the drill is clamped.
What you see
The hole wall is scored, torn or rough instead of smooth.
Causes and what to change
Every fix here is from OSG's troubleshooting guide, unless marked. Change one thing at a time.
A regrind that left wear on the drill
Regrind until all the wear is gone
Coolant that doesn’t reach the point, or too little of it
Change how coolant reaches the point, and raise its volume
Runout at the holder, or a drill not held tight
Check runout at the holder, or use another holder, and check again once the drill is clamped
Feed too high
Lower the feed
Work it out: Drilling speeds and feeds calculator
A worn drill, or metal building up on the margins
Regrind the drill, or use a coated drill
Chips packing in the flutes
Use a drill made to clear chips (wide flute, high helix or coolant through), or peck the hole
Work it out: Drilling speeds and feeds calculator
Work it out
Often comes with
Sources
Sources1
Written in our own words from each maker's troubleshooting guide.