Holes come out undersize
Mitsubishi says: use a drill with coolant through the tool; raise the coolant flow; lower the cutting speed.
What you see
The hole measures small, often after the drill has run hot.
Causes and what to change
Every fix here is from Mitsubishi's troubleshooting guide, unless marked. Change one thing at a time.
Too much heat in the cut
Use a drill with coolant through the tool
Too little coolant
Raise the coolant flow
Cutting speed too high
Lower the cutting speed