Oversize or out-of-round holes
Mitsubishi and OSG both say: regrind the point so both lips match, and check it after grinding.
What you see
The hole measures large or out of round, and a gauge pin drops through loose.
Causes and what to change
Every fix here is from Mitsubishi and OSG's troubleshooting guides, unless marked. Change one thing at a time.
A point ground unevenly: lip heights that differ, or a chisel edge off center
Regrind the point so both lips match, and check it after grinding
Runout at the holder, or a drill not held tight in it
Check runout at the holder, or use another holder, and check again once the drill is clamped
Only OSG
Flutes longer than the hole needs
Use a drill with shorter flutes
Only Mitsubishi
Feed too high
Lower the feed
Only OSG
Work it out: Drilling speeds and feeds calculator
Too little lubrication at the point
Use a drill with coolant through the tool
Only OSG
Also named as causes
The guides name these, but give no change for them.
- Work not held rigidly
Work it out
Often comes with
Sources
Sources2
- Mitsubishi Materials — Drilling course: Trouble shooting
- OSG — Drilling Technical Guide, Part 8: Troubleshooting (pp. 34–35)
Written in our own words from each maker's troubleshooting guide.