Burrs
Sandvik and Mitsubishi both say: use a sharper insert: positive, PVD-coated or ground; raise the feed if it is too light for the edge’s rounding; fix notch wear: a harder grade, or vary the depth of cut.
What you see
A ragged lip where the tool enters or leaves the cut, or along the depth-of-cut line.
Causes and what to change
Every fix here is from Sandvik and Mitsubishi's troubleshooting guides, unless marked. Change one thing at a time.
An edge too dull or too rounded for the feed
Use a sharper insert: positive, PVD-coated or ground
Most of all at feeds under .004 IPR (0.1 mm/rev).
Raise the feed if it is too light for the edge’s rounding
Notch wear or chipping at the depth of cut
Fix notch wear: a harder grade, or vary the depth of cut
Cutting straight off an edge
Chamfer or radius in and out of the cut
Only Sandvik
Other changes the makers name
Turn the coolant on
Only Mitsubishi
Work it out
- Surface finish calculator· the feed an Ra callout allows
- Turning speeds and feeds calculator· a starting speed, feed and depth for your insert
Often comes with
Sources
Sources3
- Sandvik Coromant — Troubleshooting in turning (archived Dec 4, 2024)
- Mitsubishi Materials — Trouble shooting for turning (archived Jul 10, 2026)
- Mitsubishi Materials — Causes of tool damage (types of cutting edge damage and solutions)
Written in our own words from each maker's troubleshooting guide.